Paper-based Sensing Devices for Point-of- care Testing: Current Advances

João Vitor Fernandes Paiva,1 Danielly Santos Rocha,1 Daniel Santos de Paula,1 Lívia Flório Sgobbi,1 and Wendell K. T. Coltro1,2,3*

1Instituto de Química, Universidade Federal de Goiás, 74690-900, Goiânia, GO, Brazil
2Innovation Hub in Point-of-Care Technologies, 74690-900, Goiânia, GO, Brazil
3Instituto Nacional de Ciência e Tecnologia de Bioanalítica, 13084-971, Campinas, SP, Brazil

Material Matters™ 2024, 19.1

Introduction

The development of sensing platforms for promoting rapid, inexpensive, and accurate clinical diagnostics that can be used in point-of-care testing (POCT) has received noticeable attention in recent years.1 A wide range of devices designed in varied materials have been reported in the literature for multiple purposes associated with clinical screening and detection of target analytes. Among them, cellulosic paper-based substrates have emerged as simple, biocompatible, affordable, and easy-to-use platforms for POCT applications. The attractive features of this material make it a potential candidate for the development of commercial POCT devices, as it is already seen for pregnancy, Dengue, and COVID-19 diagnostic kits, which can be found in drug stores worldwide.2,3

The increasing popularity of paper platforms for POCT applications can be attributed to the inherent advantages of cellulosic material. Due to the paper porosity, the fluid can be handled spontaneously by capillary action, eliminating the need for external instruments for fluid pumping. In addition, paper is commercially available in different formats, ranging from pore size to substrate thickness, which directly affects flow rate. Knowledge of substrate properties is essential for a rational selection of the best material for the desired application since they play a crucial role in analytical performance.4

Paper-based platforms can be manufactured through different fabrication protocols, promoting the creation of microfluidic channels interconnected with detection zones for colorimetric readouts or conductive tracks for electrochemical sensing. Colorimetric and electrochemical detection are the most popular detectors associated with paper-based devices. Colorimetric detection can be performed by the naked eye, allowing rapid yes- or-no responses, which greatly appeals to POCT applications. However, the colorimetric readout is quantified by extracting the color intensity of a digitalized image using specific software or free applications (Apps). This opens the possibility of exploring portable scanners or smartphones for supporting quantitative analysis when required. In the same way, electrochemical measurement may be done using portable and battery-powered potentiostats that are compatible with smartphones and tablets, making their use possible in the POCT.1,5

Considering the immense potential of paper-based sensing devices for POCT and commercialization,4 this mini-review summarizes the up-to-the-minute advances in clinical diagnostics. A summary of the most common protocols for fabricating paper-based sensing platforms and very recent examples of clinical diagnostics are successfully presented and discussed.

Fabrication Techniques of Paper-based Sensors and Biosensors

Various fabrication methods of colorimetric or electrochemical paper-based analytical devices (PADs) for POCT are displayed in Figure 1.

The image provides a comprehensive summary of the most common techniques for the fabrication of paper-based analytical devices. These techniques include sol-gel, stamping, laser cutting, wax techniques, inkjet printing, screen printing, permanent marker pen, eyeliner pencil, cutter printer, lithography, scholar glue, and 3D printing. This summary offers a valuable overview of the diverse methods available for the fabrication of paper-based analytical devices, catering to various requirements such as precision, scalability, material compatibility, and cost-effectiveness. The visual representation enhances the understanding of these fabrication techniques, providing researchers and practitioners with a resourceful reference for the development and optimization of paper-based analytical devices for a wide range of applications.

Figure 1.Summary of the most common techniques for the fabrication of paper-based analytical devices. Reproduced with permission from reference 26, copyright Springer 2014.

The colorimetric PADs include lateral flow assays (LFAs) and microfluidic PADs (μPADs). The formation of a hydrophobic boundary in μPADs is crucial to attaining a physical barrier for the sample distribution pathway toward detection zones. Its popularity is associated with the mass production of highly reproducible devices. The most common procedures to fabricate physical barriers are those based on wax techniques, such as wax printing5–8 and inkjet.9 In wax printing, a solid ink printer is used to delimit hydrophobic barriers on the paper’s surface. Applying hot lamination increases the wax’s permeability in the paper’s pores, improving insulation. Afterward, the reaction zone is impregnated with specific colorimetric reagents (chromogens) to interact with the target present in the sample, thus producing changes in the coloration.

In the case of LFA, the test and control lines are prepared using the streptavidin-biotin interaction10–12 principle to promote the conjugation with the recognition element that will further interact with the target.

Regarding electrochemical paper-based analytical device (ePAD) fabrication, the techniques most commonly used to manufacture ePADs are wax printing, screen printing, and stencil printing.13–15 Filter paper and Whatman® chromatography paper substrates are commonly used due to their versatility, porosity, flexibility, and robustness. Screen printing and stencil printing are employed to fabricate electrochemical biosensor electrodes. Conductive ink is applied to the substrate by squeezing it through a fine mesh screen or stencil mold, printing the paper surface.16 These technologies allow the mass production of cost-effective electrodes, enabling system miniaturization and reducing the sample volume for analysis. Automated production minimizes the issues related to the lack of reproducibility.

Materials and Practical Applications

Several ink formulations can be proposed, considering different solvent, binder, and conductive compound compositions for each specific application. Silva-Neto and collaborators17 created conductive ink using graphite flakes and waste acrylonitrile- butadiene-styrene (ABS) filaments used in 3D printing. The conductive ink was used in the confection of electrodes by stencil printing to make a paper-based electrochemical sensor to analyze S-nitroso-cysteine.

However, there are other methods of making even simpler electrodes. For instance, Souza et al.18 reported using graphite ink and nail polish on filter paper. Despite the easy and low-cost production of this electrode, large-scale manufacturing may be impractical due to the non-uniform application of conductive ink with a brush. However, to solve this problem, the authors polished the electrode and observed an increase in sensitivity.

With the electrodes manufactured, the next step is to modify the surface of the working electrode through electrodeposition, drop casting, and dipping with elements of target recognition, mediators, and receptors. This procedure is critical to improving the selectivity and sensitivity of the biosensor for biomarkers of clinical interest.19 For modification, compounds responsible for sample recognition and improvement of electron transfer are used, such as enzymes, aptamers, peptide nucleic acids, metallic nanoparticles, nanocomposites, monoclonal antibodies, metallic oxides, carbon nanotubes (Cat. Nos. 901046, 901019, 901634), polymers, antigens, Nafion™, carbon dots (Cat. Nos. 900726, 900713), etc.8,15,20

Gupta and Ghrera,20 synthesized a nanocomposite capable of transforming paper into a conductor to manufacture electrodes. The paper was dipped in a mix of polystyrene sulfonate (PEDOT:PSS, Cat. Nos. 483028, 900208, 900181) and gold nanoparticles and ultrasonicated for 40 min, promoting the deposition of PEDOT:PSS-AuNP on the cellulose fibers. Then, for the functionalization of the electrode to detect the biomarker procalcitonin, a monoclonal antibody (anti-PCT) and a blocking agent, BSA, were dropped over the working electrode. When anti- PCT and BSA were added, the peak current decreased due to the insulating characteristic of BSA, which reduced the transfer of electrons between the electrode-solution interface.

Due to the global COVID-19 outbreak, there was a need to develop devices capable of detecting the virus and assisting in monitoring and identifying infected people. Based on this, many efforts have been devoted to the development of ePADs capable of detecting SARS-CoV-2 using different bioreceptors, such as pyrrolidinyl peptide nucleic acid (acpcPNA), monoclonal antibody (mAb) CR3022 and complementary DNA (cDNA).22–24

For the fabrication of a DNA biosensor for COVID-19, Lomae et al.25 first demonstrated cellulose oxidation using a periodate solution, which resulted in the formation of aldehyde groups on the paper surface. Next, they synthesized an acpcPNA capable of binding to the SARS-CoV-2 cDNA. The ePAD functionalization occurred after a solution with acpcPNA and NaBH3CN in dimethylformamide (DMF, Cat. No. 5.89565) was dropped over the aldehyde-modified paper, promoting the immobilization of acpcPNA via covalent bonding.

POCT Applications Using Paper-based Devices

In recent years, POCT devices have emerged as powerful platforms for clinical analysis.27 Some advantages inherent to using such analytical devices are portability, ease of use, disposability (often environmentally friendly), rapid responses, accuracy, sensitivity comparable to more sophisticated techniques, and affordable costs. Additionally, because patients can frequently explore POCT platforms, they can help decentralize tests that are routinely conducted in hospitals and specialty clinics. In this sense, clinical analysis at the point of care plays a crucial role in assisting in the control of disease in the event of an epidemic or pandemic and in promoting early diagnosis and treatment.27,28

COVID-19 Diagnosis

Coronavirus disease 2019 (COVID-19) is caused by the severe acute respiratory syndrome coronavirus 2 (SARS-CoV-2) virus. Symptoms related to the SARS-CoV-2 infection range from cough and fever in simpler cases to more severe cases that can progress to pneumonia and death. One of the crucial characteristics of SARS-CoV-2 is its high level of transmissibility, which culminated in late 2019 in a pandemic that resulted in the deaths of more than 6 million people to date.29 Therefore, the rapid discovery of the SARS-CoV-2 infection is extremely important to initiate prompt treatment and prevent more people from being contaminated.

Regarding COVID-19 diagnosis, Reverse Transcriptase Polymerase Chain Reaction (RT-PCR) is considered a gold standard technique and presents the lowest limits of detection (LODs) and high specificity for results. However, RT-PCR is classified as a high-cost technology. On the other hand, employing analytical platforms for SARS-CoV-2 detection at the point-of-care proves to be an efficient and cost-effective approach. It enables rapid delivery of results, even in the initial stages of infection, including in asymptomatic patients. Some common examples of COVID-19 diagnostic devices developed considering paper platforms in 2023 are lateral flow immunoassay devices, colorimetric sensors (spot-test or microfluidics), and electrochemical devices. Some examples of these are mentioned in the next sections.28

Lateral Flow Immunoassay Devices

Recently, Lee et al.30 developed a colorimetric lateral flow immunoassay (LFIA) based on oriented antibody immobilization for rapid, accurate, sensitive, and early detection of SARS-CoV-2 trough receptor binding domain (RBD) (See Figure 2). Some materials, such as cellulose membrane and absorbent pads, were successfully used for fabricating the analytical device. For this purpose, a CBP31-BC bio-functional linker was used to immobilize antibody-conjugated gold nanoparticles (AuNPs, Cat. Nos. 928070, 928186, 927856, and 928194) on a cellulose membrane, recognizing the antigens to form antigen-antibody complexes—the proposed LFIA presents visual detection of SARS-CoV-2 in 15 min. The relationship of RBD concentrations ranging from 0.05 to 200 ng mL-1 was analyzed. The appreciable limit of detection (LOD) was estimated to be equal to 5 × 104 copies mL-1.

To verify the applicability of the device, 19 real nasopharyngeal samples were analyzed along side healthy samples, then compared to RT-PCR results, which demonstrated 100% accuracy (including samples with low viral loads). The results presented the proposed analytical platform as a rapid and accurate strategy to promote point-of-care testing to control COVID-19 proliferation.

The image presents a schematic illustration of the CBP31-BC-based lateral flow immunoassay (LFIA) designed for the detection of SARS-CoV-2. The visualization highlights the workflow of the assay, where the sample containing SARS-CoV-2 is applied to the sample pad, travels through the conjugate pad, and migrates down a cellulose membrane. Upon binding to the test line, a positive result is indicated. This schematic provides valuable insights into the design and operational principles of the LFIA, offering a clear depiction of the assay's workflow and the molecular interactions involved in detecting SARS-CoV-2. The visual representation enhances understanding of the LFIA platform, contributing to advancements in point-of-care diagnostics and infectious disease monitoring.

Figure 2.Schematic illustration of the CBP31-BC-based LFIA for detecting SARS-CoV-2. Reproduced with permission from reference 30, copyright Elsevier 2023.

Microfluidic Devices

Recently, Li et al.9 successfully proposed a rotational paper-based sensing platform coupled with a tetrahedral DNA framework (TDF) for discriminating between SARS-CoV-2 and influenza A H1N1 virus (Figure 3 A–C). Regarding the construction of the device, Whatman filter paper was wax-printed and heated to create the hydrophobic barrier. Posteriorly, the reaction between horseradish peroxidase (HRP) and 3,3′,5,5′-tetramethylbenzidine (TMB)–H2O2 was explored. Thus, the color change obtained by colorimetric response was analyzed in grayscale using free ImageJ software. Spike protein and H1N1 were detected with adequate sensitivity, considering the buffer and swab virus preservation solution matrix. Therefore, the portable, low-cost, and disposable device provided a reliable method for rapid clinical differentiation and diagnosis of COVID-19 and influenza A.

The image presents a graphical representation of a paper analytical device designed for the detection of SARS-CoV-2. It depicts the two layers of the device, with the upper detection layer featuring a reaction zone (hydrophilic area) and a hydrophobic barrier, while the lower washing layer includes a hydrophobic barrier and a washing channel. The two layers are held together by a rivet, creating the full device. This visual representation provides valuable insights into the design and structural elements of the paper analytical device, offering a clear depiction of the device's components and assembly, which are crucial for its functionality in detecting SARS-CoV-2.
The schematic illustrates the working process of the analytical device, showcasing the difference between the detection and washing functions, which are controlled by rotating the washing layer. This visualization offers a clear understanding of the operational principles of the device, particularly the mechanism for transitioning between the detection and washing phases. The schematic effectively communicates how the device's components and design enable the controlled manipulation of fluids, contributing to the accurate and reliable detection of SARS-CoV-2 and other analytes.
The image presents an analytical procedure for the detection of S protein and H1N1 using a paper analytical device. This procedure offers insights into the device's application for detecting specific antigens, highlighting its versatility and potential for multiplexed analysis of different analytes. The visual representation of the analytical procedure enhances understanding of the device's capabilities, providing valuable information for its use in rapid and specific detection of infectious agents and biomolecules.

Figure 3.Microfluidic device to detect SARS-CoV-2. A) Graphical representation of paper analytical device. B) Schematic of the working process of analytical device composed by “detection/washing” controlled by rotating the washing layer. C) Analytical procedure for detecting of S protein and H1N1. Reproduced with permission from reference 25, copyright 2023 Elsevier.

Electrochemical Devices

Lomae et al.25 manufactured a novel disposable paper-based electrochemical sensor for detecting SARS-CoV-2 (Figure 4A) using Whatman chromatography paper as the substrate. For electrode construction, graphene conductive ink (Cat. Nos. 900450, 900695, 900960) and silver/silver chloride (Ag/AgCl, Cat. Nos. 901090, 923575, 907669, 923559, 923567) ink were explored. The strategy used consisted of a working electrode (WE) modification using pyrrolidinyl peptide nucleic acid (acpcPNA) as the biological recognition element to capture the target complementary DNA (cDNA). In this sense, the electrochemical response provided by a redox probe decreased in the presence of the target cDNA since hybridization with acpcPNA promotes a block of the WE surface. This way, the electrochemical readout was correlated to SARS-CoV-2 concentration. It is important to mention that the proposed method was explored using a portable smartphone-assisted Sensit Smart Potentiostat (PalmSens) to record data. The PNA-based electrochemical paper-based analytical device (PNA-based ePAD) is of high specificity toward the SARS-CoV-2 N gene due to highly selective PNA-DNA binding and satisfactory detection limit (1.0 pmol L−1). Finally, the PNA- based ePAD was successfully used to promote the detection of amplification-free SARS-CoV-2 in 10 nasopharyngeal swab samples (7 positive and 3 negative), providing results with 100% agreement with results recorded using a gold technique (RT-PCR).

Jaewjaroenwattana et al.23 proposed a simple and low-cost electroanalytical platform to promote SARS-CoV-2 antigen detection (Figure 4B). For fabricating the disposable paper- based immunosensor, a plant-based anti-SARS-CoV-2 monoclonal antibody CR3022, expressed in Nicotiana benthamiana, is a cost- effective approach. To achieve effective antibody immobilization, an endeavor was made to enhance the presence of COOH functional groups on the electrode surface. This was accomplished by modifying the screen-printed graphene electrode with cellulose nanocrystals. Differential pulse voltammetry was used for the electrochemical readout provided by the [Fe(CN)6]3-/4- redox probe, allowing quantification of the presence of the receptor binding domain (RBD) spike protein of SARS-CoV-2. The proposed method provided satisfactory performance, including linearity in the concentration range from 0.1 pg mL-1 to 500 ng mL-1 and a limit of detection of 2.0 fg mL-1. The feasibility of the electrochemical immunosensor was successfully tested for detecting RBD in nasopharyngeal swab samples that were in concordance when compared with RT-PCR analysis. Moreover, different levels of RBD in spiked artificial saliva samples were tested, showing the ability of the sensor to detect the target analyte in different matrices and highlighting the potential use of the paper-based electrochemical sensor as a POCT device for COVID-19 diagnosis.

On the left, a schematic of a PNA-based ePAD, sized like a coin, with a front view showing the loading channel and encapsulated layer, and a back view highlighting the test and sample zones. On the right, a representation of electroanalytical measurement using a smartphone-based potentiostat, involving loading the sample, device assembly, and measurement by connecting to the potentiostat.
Design and the detection procedure using paper-based electrochemical immunosensor dedicated to detection of SARS-CoV-2. Steps go from sample loading, device assembly by folding, washing step and DPV measurement

Figure 4.Electrochemical detection of SARS-CoV-2. A1) Schematic representation of PNA-based ePAD. A2) Representation of electroanalytical measurement using a smartphone-based potentiostat. Reproduced with permission from reference 9, copyright 2023 Elsevier. B) Design and the detection procedure using paper-based electrochemical immunosensor dedicated to detection of SARS-CoV-2. Reproduced with permission from reference 23, copyright 2023 Elsevier.

Conclusion and Perspectives

This review provided an overview of the pocket-sized point-of-care technologies that can open many possibilities for healthcare applications with the promise of inexpensive, fast, and precise analyses. Some examples of materials employed to construct paper devices were reviewed. Chromatographic paper, carbon allotropes, gold nanoparticles, and specific antibodies are primarily suitable for biological sensing applications. Many aspects of paper-based sensors need to be developed for further progress in the field, such as the full validation of clinical trials through large-scale investigations with the fundamental collaboration of medical professionals. Considering their versatility, these devices require significant work to advance beyond prototypes into commercial use. We believe the proposed paper can be routinely employed to increase the use of paper-based devices for point-of-care testing.

Acknowledgments

The authors would like to thank CAPES (finance code 88887.192880/2018-00),  CNPq  (grants  307554/2020-1, 401256/2020-0 and 405620/2021-7), and INCTBio (grant 465389/2014-7) for the financial support and granted scholarships.

Related Products

Loading

References

1.
Silva-Neto HA, Arantes IV, Ferreira AL, do Nascimento GH, Meloni GN, de Araujo WR, Paixão TR, Coltro WK. 2023. Recent advances on paper-based microfluidic devices for bioanalysis. TrAC Trends in Analytical Chemistry. 158116893. https://doi.org/10.1016/j.trac.2022.116893
2.
Kumar A, Parihar A, Panda U, Parihar DS. 2022. Microfluidics-Based Point-of-Care Testing (POCT) Devices in Dealing with Waves of COVID-19 Pandemic: The Emerging Solution. ACS Appl. Bio Mater. 5(5):2046-2068. https://doi.org/10.1021/acsabm.1c01320
3.
Pinheiro KM, Guinati BG, Moreira NS, Coltro WK. 2023. Low-Cost Microfluidic Systems for Detection of Neglected Tropical Diseases. Annual Rev. Anal. Chem. 16(1):117-138. https://doi.org/10.1146/annurev-anchem-091522-024759
4.
Coltro W. 2022. Paper-based microfluidics: What can we expect?. Braz. J. Anal. Chem. 9(37):11-13. https://doi.org/10.30744/brjac.2179-3425.point-of-view-wktcoltro.n37
5.
Wang X, Zheng X, Song Z, Lin D, Li Q, Qi J, Xiang J, Meirong Wang, Chen L, Li B. 2023. Electric yo-yo centrifugation combining with paper-based microfluidic immunoassay chip for inflammatory biomarkers detection in whole blood. Talanta. 253123883. https://doi.org/10.1016/j.talanta.2022.123883
6.
Nguyen QH, Lee DH, Nguyen PT, Le PG, Kim MI. 2023. Foldable paper microfluidic device based on single iron site-containing hydrogel nanozyme for efficient glucose biosensing. Chemical Engineering Journal. 454140541. https://doi.org/10.1016/j.cej.2022.140541
7.
Lakshmi Devi A, Resmi P, Pradeep A, Suneesh P, Nair BG, Satheesh Babu T. 2023. A paper-based point-of-care testing device for the colourimetric estimation of bilirubin in blood sample. Spectrochimica Acta Part A: Molecular and Biomolecular Spectroscopy. 287122045. https://doi.org/10.1016/j.saa.2022.122045
8.
Cheng Y, Feng S, Ning Q, Li T, Xu H, Sun Q, Cui D, Wang K. Dual-signal readout paper-based wearable biosensor with a 3D origami structure for multiplexed analyte detection in sweat. Microsyst Nanoeng. 9(1): https://doi.org/10.1038/s41378-023-00514-2
9.
Li F, Qi J, Ren Z, Hu X, Chen Y, Li B, Fu X. 2023. Tetrahedral DNA framework assisted rotational paper-based analytical device for differential detection of SARS-CoV-2 and influenza A H1N1 virus. Microchemical Journal. 185108304. https://doi.org/10.1016/j.microc.2022.108304
10.
Çam Derin D, Gültekin E, İçen Taşkın I, Yakupoğulları Y. 2023. Development of nucleic acid based lateral flow assays for SARS-CoV-2 detection. Journal of Bioscience and Bioengineering. 135(2):87-92. https://doi.org/10.1016/j.jbiosc.2022.11.001
11.
Yang LF, Kacherovsky N, Panpradist N, Wan R, Liang J, Zhang B, Salipante SJ, Lutz BR, Pun SH. 2022. Aptamer Sandwich Lateral Flow Assay (AptaFlow) for Antibody-Free SARS-CoV-2 Detection. Anal. Chem. 94(20):7278-7285. https://doi.org/10.1021/acs.analchem.2c00554
12.
Chen P, Meng Y, Liu T, Peng W, Gao Y, He Y, Qu R, Zhang C, Hu W, Ying B. 2023. Sensitive Urine Immunoassay for Visualization of Lipoarabinomannan for Noninvasive Tuberculosis Diagnosis. ACS Nano. 17(7):6998-7006. https://doi.org/10.1021/acsnano.3c01374
13.
Shan L, Chen Y, Tan X, Ge S, Zhang L, Li L, Yu J, Li L. 2023. Tetrahedral DNA Nanostructure-Engineered Paper-Based Sensor with an Enhanced Antifouling Ability for Photoelectrochemical Sensing. Anal. Chem. 95(10):4760-4767. https://doi.org/10.1021/acs.analchem.2c05686
14.
Yang M, Sun N, Lai X, Wu J, Wu L, Zhao X, Feng L. 2023. Paper-Based Sandwich-Structured Wearable Sensor with Sebum Filtering for Continuous Detection of Sweat pH. ACS Sens. 8(1):176-186. https://doi.org/10.1021/acssensors.2c02016
15.
Hasan MR, Sharma P, Shaikh S, Singh S, Pilloton R, Narang J. Electrochemical Aptasensor Developed Using Two-Electrode Setup and Three-Electrode Setup: Comprising Their Current Range in Context of Dengue Virus Determination. Biosensors. 13(1):1. https://doi.org/10.3390/bios13010001
16.
Holman JB, Shi Z, Fadahunsi AA, Li C, Ding W. 2023. Advances on microfluidic paper-based electroanalytical devices. Biotechnology Advances. 63108093. https://doi.org/10.1016/j.biotechadv.2022.108093
17.
Silva-Neto HA, Duarte-Junior GF, Rocha DS, Bedioui F, Varenne A, Coltro WKT. Recycling 3D Printed Residues for the Development of Disposable Paper-Based Electrochemical Sensors. ACS Appl. Mater. Interfaces. https://doi.org/10.1021/acsami.3c00370
18.
de Souza CC, Lisboa TP, de Oliveira WBV, Abarza Muñoz RA, Costa Matos MA, Matos RC. 2023. Simple strategy for the detection of the amoxicillin antibiotic in different matrices using a low-cost paper electrode. Talanta. 253124050. https://doi.org/10.1016/j.talanta.2022.124050
19.
Kim ER, Joe C, Mitchell RJ, Gu MB. 2023. Biosensors for healthcare: current and future perspectives. Trends in Biotechnology. 41(3):374-395. https://doi.org/10.1016/j.tibtech.2022.12.005
20.
Mazzaracchio V, Bagheri N, Chiara F, Fiore L, Moscone D, Roggero S, Arduini F. 2023. A smart paper-based electrochemical sensor for reliable detection of iron ions in serum. Anal Bioanal Chem. 415(6):1149-1157. https://doi.org/10.1007/s00216-023-04537-6
21.
Gupta Y, Ghrera AS. Development of conducting paper-based electrochemical biosensor for procalcitonin detection. ADMET DMPK. https://doi.org/10.5599/admet.1575
22.
Farzin MA, Abdoos H, Saber R. 2022. AuNP-based biosensors for the diagnosis of pathogenic human coronaviruses: COVID-19 pandemic developments. Anal Bioanal Chem. 414(24):7069-7084. https://doi.org/10.1007/s00216-022-04193-2
23.
Jaewjaroenwattana J, Phoolcharoen W, Pasomsub E, Teengam P, Chailapakul O. 2023. Electrochemical paper-based antigen sensing platform using plant-derived monoclonal antibody for detecting SARS-CoV-2. Talanta. 251123783. https://doi.org/10.1016/j.talanta.2022.123783
24.
Ong V, Soleimani A, Amirghasemi F, Khazaee Nejad S, Abdelmonem M, Razaviyayn M, Hosseinzadeh P, Comai L, Mousavi MPS. Impedimetric Sensing: An Emerging Tool for Combating the COVID-19 Pandemic. Biosensors. 13(2):204. https://doi.org/10.3390/bios13020204
25.
Lomae A, Preechakasedkit P, Hanpanich O, Ozer T, Henry CS, Maruyama A, Pasomsub E, Phuphuakrat A, Rengpipat S, Vilaivan T, et al. 2023. Label free electrochemical DNA biosensor for COVID-19 diagnosis. Talanta. 253123992. https://doi.org/10.1016/j.talanta.2022.123992
26.
Taleat Z, Khoshroo A, Mazloum-Ardakani M. 2014. Screen-printed electrodes for biosensing: a review (2008–2013). Microchim Acta. 181(9-10):865-891. https://doi.org/10.1007/s00604-014-1181-1
27.
Luppa PB, Müller C, Schlichtiger A, Schlebusch H. 2011. Point-of-care testing (POCT): Current techniques and future perspectives. TrAC Trends in Analytical Chemistry. 30(6):887-898. https://doi.org/10.1016/j.trac.2011.01.019
28.
Song Q, Sun X, Dai Z, Gao Y, Gong X, Zhou B, Wu J, Wen W. Point-of-care testing detection methods for COVID-19. Lab Chip. 21(9):1634-1660. https://doi.org/10.1039/d0lc01156h
29.
WHO Coronavirus (COVID-19) Dashboard. [Internet]. WHO Coronavirus (COVID-19) Dashboard With Vaccination Data. . Available from: https://data.who.int/dashboards/covid19/cases?n=c
30.
Lee AS, Kim SM, Kim KR, Park C, Lee D, Heo HR, Cha HJ, Kim CS. 2023. A colorimetric lateral flow immunoassay based on oriented antibody immobilization for sensitive detection of SARS-CoV-2. Sensors and Actuators B: Chemical. 379133245. https://doi.org/10.1016/j.snb.2022.133245