偏硼酸锂

99.995% trace metals basis

别名:

硼酸锂盐

登录 查看组织和合同定价。

选择尺寸


关于此项目

线性分子式:
LiBO2
化学文摘社编号:
分子量:
49.75
NACRES:
NA.23
PubChem Substance ID:
UNSPSC Code:
12352302
EC Number:
236-631-5
MDL number:
Assay:
99.995% trace metals basis
Form:
powder
技术服务
需要帮助?我们经验丰富的科学家团队随时乐意为您服务。
让我们为您提供帮助
技术服务
需要帮助?我们经验丰富的科学家团队随时乐意为您服务。
让我们为您提供帮助

产品名称

偏硼酸锂, 99.995% trace metals basis

InChI key

HZRMTWQRDMYLNW-UHFFFAOYSA-N

InChI

1S/BO2.Li/c2-1-3;/q-1;+1

SMILES string

[Li+].[O-]B=O

assay

99.995% trace metals basis

form

powder

reaction suitability

core: lithium

impurities

≤55.0 ppm Trace Metal Analysis

mp

845 °C (lit.)

application(s)

battery precursors
catalysts
material synthesis precursor

Quality Level

正在寻找类似产品? 访问 产品对比指南

signalword

Danger

Hazard Classifications

Acute Tox. 4 Oral - Eye Dam. 1 - Repr. 2

存储类别

13 - Non Combustible Solids

wgk

WGK 1

flash_point_f

Not applicable

flash_point_c

Not applicable

ppe

Eyeshields, Gloves, type N95 (US)


历史批次信息供参考:

分析证书(COA)

Lot/Batch Number

没有发现合适的版本?

如果您需要特殊版本,可通过批号或批次号查找具体证书。

已有该产品?

在文件库中查找您最近购买产品的文档。

访问文档库

Jing-lin You et al.
Guang pu xue yu guang pu fen xi = Guang pu, 22(5), 787-789 (2003-08-27)
Raman spectra of xCaSiO3.LiBO2 (by weight ratio, x = 0, 0.25, 0.33, 0.50) crystals were measured. The microstructure of different silicon-oxygen tetrahedrons and their abundant variations with silica contents were studied. It shows that all the silicon-oxygen tetrahedrons are isolated
S Miljanić et al.
Radiation protection dosimetry, 119(1-4), 191-196 (2006-05-20)
Recently, two new types of 'tissue equivalent' thermoluminescent detectors (TLDs) have aroused attention: LiF:Mg,Cu,Na,Si and Li2B4O7:Cu,Ag,P. In this work the characteristics of both detectors were compared with the characteristics of the well-known type LiF:Mg,Ti detector, TLD-100. The following properties were
Thomas Hermanns et al.
The Journal of urology, 185(6), 2241-2247 (2011-04-19)
Technical modifications of the 120 W lithium-triborate laser have been implemented to increase power output, and prevent laser fiber degradation and loss of power output during laser vaporization of the prostate. However, visible alterations at the fiber tip and the
M Ceretti et al.
Radiation protection dosimetry, 144(1-4), 262-265 (2011-02-08)
This work summarises the results of a series of experiences made on Panasonic UD-802AS, a multi-element dosemeter that is currently used in Caorso Nuclear Power Plant for personnel external monitoring. Two main topics have been considered: energy response and the
Frank R Wagner et al.
Optics express, 18(26), 26791-26798 (2011-01-05)
Multiple pulse nanosecond laser induced damage in the bulk of LiB3O5 (LBO) crystals was investigated at 1064 nm, 532 nm and 355 nm. Scanning electron microscopy of cleaved damage sites confirmed the presence of different zones that have already been