form
solid
Quality Segment
feed ratio
NIPAM:BA 20:1
mol wt
average Mn 30,000
composition
butylacrylate, 5 mol %
transition temp
LCST 25 °C, Tm 345-351
Application
This copolymer shows LCST at 25°C (lower temperature than PolyNIPAM), which makes it useful in hydrogel and tissue engineering applications needing LCST close to room temperature or below.