Quality Level
assay
98% trace metals basis
form
nanofiber
D
<2.5 μm
mp
2700 °C (lit.)
density
3.22 g/mL at 25 °C (lit.)
SMILES string
[C-]#[Si+]
InChI
1S/CSi/c1-2
InChI key
HBMJWWWQQXIZIP-UHFFFAOYSA-N
Application
Silicon carbide nanofibers are used with aluminum metal ceramic composites and ceramic composites to increase strength and reduce stress. Silicon carbide nanowhiskers can also be used in biocomposites for bone repair.
Still not finding the right product?
Explore all of our products under 碳化硅
signalword
Danger
hcodes
Hazard Classifications
Carc. 1B Inhalation
存储类别
6.1D - Non-combustible acute toxic Cat.3 / toxic hazardous materials or hazardous materials causing chronic effects
wgk
nwg
flash_point_f
Not applicable
flash_point_c
Not applicable
商品
Controlled synthesis of metal clusters regulates ligands and atoms, advancing metal nanomaterial synthesis.
Catalytic water splitting produces hydrogen crucial for renewable energy, petroleum refining, and chemical industry applications like methanol production.
TiO2 exhibits wide band gap semiconductor and memristor properties electronically, with high opacity and UV absorbance optically.
Fabrication of Mullite and Mullite-Matrix Composites by Transient Viscous Sintering of Composite Powders
Sacks, M.D.; Bozkurt, N.; Scheiffele, G.W.;
Journal of the American Ceramic Society. American Ceramic Society, 74(10), 2428-2437 (1991)
Hockin H K Xu et al.
Biomaterials, 25(19), 4615-4626 (2004-05-04)
Self-hardening calcium phosphate cement (CPC) sets to form hydroxyapatite with high osteoconductivity, but its brittleness and low strength limit its use to only non-stress bearing locations. Previous studies developed bioactive composites containing hydroxyapatite fillers in Bis-GMA-based composites for bone repair
Strengthening of composites due to microstructural changes in the matrix
Arsenault, R. J.; Wang, L.; Feng, C. R.
Acta Metallurgica et Materialia, 39(1), 47-57 (1991)
全球贸易项目编号
| 货号 | GTIN |
|---|---|
| 776742-25G | 04061832940458 |