线性分子式:
Ca(NO3)2 · 4H2O
化学文摘社编号:
分子量:
236.15
NACRES:
NB.24
PubChem Substance ID:
UNSPSC Code:
12352300
EC Number:
233-332-1
MDL number:
Assay:
99%, 99.0-103.0% (ACS specification)
Grade:
ACS reagent
Form:
flakes, powder, crystals or granules
grade
ACS reagent
Quality Level
assay
99%, 99.0-103.0% (ACS specification)
form
flakes, powder, crystals or granules
impurities
≤0.005% insolubles
pH
5.0-7.0 (25 °C, 5%)
mp
44 °C (dec.) (lit.)
density
1.86 g/mL at 25 °C
anion traces
chloride (Cl-): ≤0.005%, nitrite (NO2-): ≤0.001%, sulfate (SO42-): ≤0.002%
cation traces
Ba: ≤0.005%, Fe: ≤5 ppm, K: ≤0.005%, Mg: ≤0.05%, Na: ≤0.01%, Sr: ≤0.05%, heavy metals: ≤5 ppm (by ICP-OES)
SMILES string
O.O.O.O.[Ca++].[O-][N+]([O-])=O.[O-][N+]([O-])=O
InChI
1S/Ca.2NO3.4H2O/c;2*2-1(3)4;;;;/h;;;4*1H2/q+2;2*-1;;;;
InChI key
ICSSIKVYVJQJND-UHFFFAOYSA-N
General description
硝酸钙四水合物是一种无机化合物,可用于冷却浴和废水处理。
Application
硝酸钙四水合物被用作:
与钾前体磷酸二氢钾一起在通过溶胶-凝胶沉淀法合成纳米羟基磷灰石(HA)颗粒中作为钙前体。
作为前驱体与磷酸氢二铵一起用于通过湿化学技术合成纳米羟基磷灰石(n-HAP)。
在58S生物活性玻璃的制备中,该玻璃的成分由三元系统SiO2 (58 wt%) - CaO (33 wt%) - P2O5 (9wt%)组成。
与钾前体磷酸二氢钾一起在通过溶胶-凝胶沉淀法合成纳米羟基磷灰石(HA)颗粒中作为钙前体。
作为前驱体与磷酸氢二铵一起用于通过湿化学技术合成纳米羟基磷灰石(n-HAP)。
在58S生物活性玻璃的制备中,该玻璃的成分由三元系统SiO2 (58 wt%) - CaO (33 wt%) - P2O5 (9wt%)组成。
Still not finding the right product?
Explore all of our products under 硝酸钙 四水合物
signalword
Danger
hcodes
Hazard Classifications
Acute Tox. 4 Oral - Eye Dam. 1
存储类别
13 - Non Combustible Solids
flash_point_f
Not applicable
flash_point_c
Not applicable
法规信息
易制爆化学品
危险化学品
此项目有
Joana Moreira et al.
Molecules (Basel, Switzerland), 25(4) (2020-02-23)
Freestanding films based on catechol functionalized chitosan (CHI), hyaluronic acid (HA), and bioglass nanoparticles (BGNPs) were developed by spin-coating layer-by-layer assembly (SA-LbL). The catechol groups of 3,4-dihydroxy-l-phenylalanine (DOPA) present in the marine mussels adhesive proteins (MAPs) are the main factors
Breno R Barrioni et al.
Journal of colloid and interface science, 547, 382-392 (2019-04-12)
Bioactive glass nanoparticles (BGNPs) are of great interest in tissue engineering as they possess high dissolution rate and capability of being internalized by cells, releasing their dissolution products with therapeutic benefits intracellularly. A modified Stöber process can be applied to
Eagleson M.
Concise Encyclopedia Chemistry, 164-164 (1994)
全球贸易项目编号
| 货号 | GTIN |
|---|---|
| SML0429-5MG | 04061833222805 |
| SML0429-1MG | 04061838037824 |
| 400012-5MG | 07790788049928 |
| 237124-500G | 04061838785992 |
| 237124-2.5KG | 04061838785985 |