登录 查看组织和合同定价。
选择规格
变更视图
关于此项目
线性分子式:
LiCl
化学文摘社编号:
分子量:
42.39
NACRES:
NA.23
PubChem Substance ID:
UNSPSC Code:
12352302
EC Number:
231-212-3
MDL number:
Assay:
99.998% trace metals basis
Grade:
synthesis grade
Form:
beads
Solubility:
H2O: soluble
grade
synthesis grade
Quality Segment
product line
AnhydroBeads™
assay
99.998% trace metals basis
form
beads
reaction suitability
core: lithium
greener alternative product characteristics
Design for Energy Efficiency
Learn more about the Principles of Green Chemistry.
sustainability
Greener Alternative Product
impurities
≤25.0 ppm Trace Metal Analysis
particle size
−10 mesh
mp
605 °C (lit.)
solubility
H2O: soluble
application(s)
battery precursors
catalysts
electroplating
material synthesis precursor
greener alternative category
SMILES string
[Li+].[Cl-]
InChI
1S/ClH.Li/h1H;/q;+1/p-1
InChI key
KWGKDLIKAYFUFQ-UHFFFAOYSA-M
General description
氯化锂是一种无水锂盐,极易溶于水等极性溶剂,具吸湿性。LiCl可用作锂离子电池的电解质添加剂,提高电池的性能和稳定性。还用于多个材料科学领域,包括生产锂金属、干燥剂、固态电解质、气体传感器、催化与有机合成。
我们竭诚为您带来符合一项或多项绿色化学12项原则要求的绿色替代产品。该产品为增强型,提高了能源效率。点击此处以获取更多信息。
我们竭诚为您带来符合一项或多项绿色化学12项原则要求的绿色替代产品。该产品为增强型,提高了能源效率。点击此处以获取更多信息。
Application
氯化锂可用于:
- 锂基金属电池中的熔融盐电解质。LiCl 促进电池充电和放电周期中电极之间锂离子的运输。LiCl和KCl对于熔融盐电解质的离子电导性和稳定性有贡献。
- 作为前体材料,开发用于高电压固相锂离子电池的氟取代氯化锂固态电解质。
- 作为盐添加剂,用于准固态染料敏化太阳能电池中电池凝胶电解质的形成。LiCl 提高了凝聚电解质的离子电导性,促进电荷在太阳能电池中的运动
- N-I-P型单片钙钛矿/硅叠层太阳电池中复合材料电子运输层开发中的添加剂。它也可加入氧化锡(SnO2) 前体溶液,钝化SnO2 层中的缺陷 ,并增进电子传输层(ETL)和钙钛矿之间界面的电子注入驱动力。
- 熔融盐反应器中的冷却剂
Legal Information
AnhydroBeads is a trademark of Sigma-Aldrich Co. LLC
Still not finding the right product?
Explore all of our products under 氯化锂
signalword
Warning
hcodes
Hazard Classifications
Acute Tox. 4 Oral - Eye Irrit. 2 - Skin Irrit. 2
flash_point_f
Not applicable
flash_point_c
Not applicable
ppe
dust mask type N95 (US), Eyeshields, Gloves
存储类别
11 - Combustible Solids