Polystyrene-block-poly(ethylene-ran-butylene)-block-polystyrene, sulfonated, cross-linkable solution
Select a Size
About This Item
composition
styrene, 29 wt. %
sulfonated styrene units, 55-56%
vinyl silane cross-linking agent, <0.5%
greener alternative product characteristics
Design for Energy Efficiency
Learn more about the Principles of Green Chemistry.
concentration
5 wt. % in 1-propanol and dichloroethane
conductivity
0.1078 S/cm (The ionic conductivity can increase up to 50% when heating from RT to 67°C)
density
0.800 g/mL at 25 °C
General description
Application
Preparation Note
1. Concentrate solution to 600 centapoise viscosity (typically 6-9 wt. % polymer).
2. Preheat the casting surface to 35 °C. A clean, flat PTFE-coated glass surface is recommended.
3. Secure a silicone release liner to the casting surface.
4. Place a small drop of the polymer solution on the release liner.
5. Draw the polymer solution down the release liner.
6. Dry the film for 30 min. For controlled evaporation it is recommended to cover surface with aluminum foil that has been perforated with small pinholes.
Signal Word
Danger
Hazard Statements
Precautionary Statements
Hazard Classifications
Carc. 1B - Eye Dam. 1 - Flam. Liq. 2 - Skin Sens. 1 - STOT SE 3
Target Organs
Respiratory system
Storage Class Code
3 - Flammable liquids
WGK
WGK 3
Flash Point(F)
51.8 °F - closed cup
Flash Point(C)
11 °C - closed cup
Personal Protective Equipment
Regulatory Information
Choose from one of the most recent versions:
Already Own This Product?
Find documentation for the products that you have recently purchased in the Document Library.
Our team of scientists has experience in all areas of research including Life Science, Material Science, Chemical Synthesis, Chromatography, Analytical and many others.
Contact Technical Service