Chemical vapor deposition (CVD) and atomic layer deposition (ALD) are widely used vapor-phase techniques for fabricating semiconductor and advanced-material thin films. Choosing the right precursor is a delicate exercise in balance. Its chemical purity, volatility, thermal stability, and surface reactivity must be carefully considered, along with its delivery characteristics, by-product formation, and compatibility with the desired film and deposition process. Only when these properties work together can a precursor deliver consistent, high-quality results.

This article presents a framework with seven criteria for screening and evaluating CVD and ALD precursors. It examines representative precursor families, including metal halides, metal alkyls, metal alkylamides, β-diketonates, carbonyls, silicon-containing precursors, and cyclopentadienyl-containing organometallics, and relates their characteristics to common thin-film applications. The framework is intended to support initial precursor selection from exploratory research through process development and scale-up.

Schematic representation of thin-film deposition processes. (1) Chemical Vapor Deposition (CVD): (1a) precursor gases enter the reactor and flow over the substrate surface, and (1b) excess gases and reaction by-products exit the reactor after film formation. (2) Atomic Layer Deposition (ALD): (2a) the first precursor adsorbs onto reactive surface sites, (2b) the surface becomes saturated through a self-limiting reaction, (2c) excess precursor and by-products are removed during the purge step, and (2d) a subsequent precursor reacts with the adsorbed layer to deposit material one atomic layer at a time, enabling uniform thin-film growth.

Figure 1.Illustration of CVD and ALD thin-film deposition mechanisms. In the CVD process (1), precursor gases enter the reactor (1a), react on the substrate surface to form a film, and exit as excess gases and by-products (1b). In the ALD process (2), the first precursor adsorbs onto the substrate (2a), saturates available surface sites through a self-limiting reaction (2b), followed by a purge step (2c), and then reacts with a second precursor to form a uniform atomic layer on the surface (2d).

Why precursor choice determines film quality in CVD and ALD?

The ideal CVD or ALD precursor is not necessarily the most volatile or the purest compound. Rather, it is one that performs reliably throughout the entire deposition process. It must remain stable during storage, vaporization, and transport; react appropriately with the substrate or co-reactant; produce the desired film composition, and satisfy the safety, equipment-compatibility, and scale-up requirements of the process.

The choice of precursor can influence nearly every aspect of film formation, including composition, growth rate, morphology, conformality, interface quality, and process reproducibility. These outcomes are governed not only by the intrinsic properties of the precursor but also by its interactions with the substrate, co-reactant, reactor, delivery system, and deposition conditions. 1-3

Precursor suitability is therefore evaluated across several interconnected criteria, including chemical purity, volatility, thermal stability, delivery behavior, surface reactivity, by-product formation, and deposition temperature. In addition, for ALD, it is also important to consider saturation behavior and the available process window whereas for a CVD, gas-phase stability and transport behavior are key factors in precursor selection.4,5

Ultimately, precursor selection is a system-level decision, the best precursor is the one that translates molecular properties into consistent, scalable, and high-quality film performance.

CVD vs. ALD: Precursor requirements by deposition mode

CVD and ALD are governed by fundamentally different growth mechanisms, and the priorities for precursor selection therefore differ between the two processes.

CVD typically focuses on efficient precursor transport, gas-phase stability, surface-reaction kinetics, deposition-rate control, and minimizing particle formation. In contrast, ALD relies on sequential, self-limiting surface reactions, making precursor saturation, purge efficiency, nucleation behavior, and the available process window particularly important.1,2

The purity panel of any precursors can help identify contaminants that may affect precursor delivery, reaction pathways, film composition, and device performance. Common specifications reviewed in lot-specific Certificates of Analysis (CoA) include those listed in Table 1. Their relevance depends on the target film and deposition chemistry.7,8

Seven key criteria for screening CVD and ALD precursors

Precursor selection is a multidimensional decision that requires careful consideration of its physical and chemical properties, process performance, safety profile, and supply availability. The seven criteria discussed in the following sections provide a structured framework for screening and evaluating precursors for CVD and ALD applications. They should be considered together with reactor design, co-reactant selection, substrate compatibility, precursor-delivery hardware, and the performance requirements of the target film. Table 2 summarizes the principal criteria used in precursor evaluation and provides a concise framework for comparing candidate materials.1,2,9-11

A selection guide to precursor class

Table 3 summarizes eight commonly used precursor families, highlighting their characteristic properties, typical deposition behavior, approximate operating-temperature ranges, and representative applications. This comparison is intended to provide an initial basis for identifying precursor classes that may be suitable for a particular film composition, deposition technique, or process requirement.

The temperature ranges given should be regarded as indicative rather than definitive. Actual deposition behavior is influenced by several interdependent factors, including precursor identity, reactor pressure, co-reactant selection, substrate characteristics, and reactor configuration. Consequently, the information in the table should be used as a guide for preliminary selection and followed by experimental evaluation under the conditions relevant to the intended process.1,2,13

Find the right precursor for your application

The following tables show key precursors for common semiconductors and advanced-material thin-film applications. They are intended to support initial screening, and not to replace process validation. The suitability of a precursor should be confirmed through delivery testing, process-window studies, film characterization, impurity analysis, and safety assessment.1,2,9 The precursor choices and important selection factors for various target films and applications are compiled in the following tables.

Key precursors for high-k gate dielectrics and memory capacitors

Disclaimer: The examples are representative starting points and should not be interpreted as universal recommendations. Suitability depends on precursor delivery, reactor configuration, substrate preparation, co-reactant chemistry, deposition conditions, and target film requirements.

Choosing the appropriate purity level

CVD and ALD precursors are available in a broad range of purity and may be accompanied by varying levels of analytical characterization. The appropriate purity level should be selected according to the intended application, required process performance, and stage of development. Beyond nominal purity, other characteristics may be equally important in assessing a precursor’s suitability for semiconductor and thin-film deposition processes. These include trace-metal purity, moisture content, the scope and quality of the analytical documentation, and the availability of lot-specific Certificate of Analysis (CoA) data. Collectively, such information provides a more complete basis for evaluating precursor quality, process compatibility, and manufacturing acceptability.7,8

Conclusion

The choice of precursors is a critical factor in CVD and ALD processes, as it can affect film quality, impurity levels, growth characteristics, process consistency, and device performance. The seven-criterion framework presented in this guide provides a structured approach for evaluating precursor suitability, while the precursor family overview and application-to-precursor navigator help identify candidate chemistries for specific thin-film applications.

The performance of a precursor is governed by a complex interplay of factors, including reactor configuration, substrate properties, co-reactant chemistry, and deposition conditions. Accordingly, no single precursor can be regarded as universally suitable for every application. The framework and selection guides presented are intended to facilitate the initial screening of candidates and support informed decision-making. Promising precursors should subsequently be subjected to systematic deposition studies, comprehensive film characterization, and process optimization. Only through this iterative evaluation can the precursor best suited to the target application and its manufacturing requirements be identified.

To explore our full range of offerings, visit our Solution and Vapor deposition Precursor webpage. 

References

1.
Kessels E, Devi A, Park J, Ritala M, Yanguas-Gil A, Wiemer C. Atomic layer deposition. Nat Rev Methods Primers. 5(1): https://doi.org/10.1038/s43586-025-00435-6
2.
Oke JA, Jen T. 2022. Atomic layer deposition and other thin film deposition techniques: from principles to film properties. Journal of Materials Research and Technology. 212481-2514. https://doi.org/10.1016/j.jmrt.2022.10.064
3.
Kilic U, Mock A, Sekora D, Gilbert S, Valloppilly S, Melendez G, Ianno N, Langell M, Schubert E, Schubert M. 2020. Precursor-surface interactions revealed during plasma-enhanced atomic layer deposition of metal oxide thin films by in-situ spectroscopic ellipsometry. Sci Rep. 10(1): https://doi.org/10.1038/s41598-020-66409-8
4.
Oh I, Sandoval TE, Liu T, Richey NE, Bent SF. 2021. Role of Precursor Choice on Area-Selective Atomic Layer Deposition. Chem. Mater.. 33(11):3926-3935. https://doi.org/10.1021/acs.chemmater.0c04718
5.
Merkx MJM, Angelidis A, Mameli A, Li J, Lemaire PC, Sharma K, Hausmann DM, Kessels WMM, Sandoval TE, Mackus AJM. 2022. Relation between Reactive Surface Sites and Precursor Choice for Area-Selective Atomic Layer Deposition Using Small Molecule Inhibitors. J. Phys. Chem. C. 126(10):4845-4853. https://doi.org/10.1021/acs.jpcc.1c10816
6.
Hagen DJ, Pemble ME, Karppinen M. 2019. Atomic layer deposition of metals: Precursors and film growth. 6(4): https://doi.org/10.1063/1.5087759
7.
Kobayashi M, Okada Y, Shirai T, Sawajiri O, Gieger R, Entezarian M. 2021. Purification Method for Achieving Low Trace Metals in Ultra-High Purity Chemicals. J. Photopol. Sci. Technol.. 34(2):205-211. https://doi.org/10.2494/photopolymer.34.205
8.
Van Acker T, Theiner S, Bolea-Fernandez E, Vanhaecke F, Koellensperger G. Inductively coupled plasma mass spectrometry. Nat Rev Methods Primers. 3(1): https://doi.org/10.1038/s43586-023-00235-w
9.
Li J, Chai G, Wang X. 2023. Atomic layer deposition of thin films: from a chemistry perspective. Int. J. Extrem. Manuf.. 5(3):032003. https://doi.org/10.1088/2631-7990/acd88e
10.
Zhang J, Li Y, Cao K, Chen R. 2022. Advances in Atomic Layer Deposition. Nanomanuf Metrol. 5(3):191-208. https://doi.org/10.1007/s41871-022-00136-8
11.
Shahmohammadi M, Mukherjee R, Sukotjo C, Diwekar U, Takoudis C. 2022. Recent Advances in Theoretical Development of Thermal Atomic Layer Deposition: A Review. Nanomaterials. 12(5):831. https://doi.org/10.3390/nano12050831
12.
Johnson AL, Parish JD. 2018. Recent developments in molecular precursors for atomic layer deposition.1-53. https://doi.org/10.1039/9781788010672-00001
13.
Zhang X, Trainor N, Mc Knight TV, Graves AR, Wu Z, Xu L, Zheng X, Zhang T, Zhu J, Palacios T, et al. 2025. Metal–organic chemical vapour deposition for 2D chalcogenides. Nat Rev Methods Primers. 5(1): https://doi.org/10.1038/s43586-025-00429-4
14.
Parsons GN, Clark RD. 2020. Area-Selective Deposition: Fundamentals, Applications, and Future Outlook. Chem. Mater.. 32(12):4920-4953. https://doi.org/10.1021/acs.chemmater.0c00722
15.
Meng X, Byun Y, Kim H, Lee J, Lucero A, Cheng L, Kim J. Atomic Layer Deposition of Silicon Nitride Thin Films: A Review of Recent Progress, Challenges, and Outlooks. Materials. 9(12):1007. https://doi.org/10.3390/ma9121007
16.
Park J, Kwak SJ, Kang S, Oh S, Shin B, Noh G, Kim TS, Kim C, Park H, Oh SH, et al. Area-selective atomic layer deposition on 2D monolayer lateral superlattices. Nat Commun. 15(1): https://doi.org/10.1038/s41467-024-46293-w
17.
Chen W, Sun Q, Xu M, Ding S, Zhang DW, Wang L. 2007. Atomic Layer Deposition of Hafnium Oxide from Tetrakis(ethylmethylamino)hafnium and Water Precursors. J. Phys. Chem. C. 111(17):6495-6499. https://doi.org/10.1021/jp070362u
18.
D’Acunto G, Tsyshevsky R, Shayesteh P, Gallet J, Bournel F, Rochet F, Pinsard I, Timm R, Head AR, Kuklja M, et al. 2023. Bimolecular Reaction Mechanism in the Amido Complex-Based Atomic Layer Deposition of HfO2. Chem. Mater.. 35(2):529-538. https://doi.org/10.1021/acs.chemmater.2c02947
19.
Kim Y, Vu MPU, Kim HJ, Park H. 2026. First-principles calculations reveal precursor-dependent reaction mechanisms in ZrO2 atomic layer deposition. Sci Rep. 16(1): https://doi.org/10.1038/s41598-026-48081-6
20.
Rose M, Niinistö J, Endler I, Bartha JW, Kücher P, Ritala M. 2010. In Situ Reaction Mechanism Studies on Ozone-Based Atomic Layer Deposition of Al2O3 and HfO2. ACS Appl. Mater. Interfaces. 2(2):347-350. https://doi.org/10.1021/am900807a
21.
Blakeney KJ, Winter CH. 2018. Thermal atomic layer deposition of tungsten carbide films from WCl6 and AlMe3. Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films. 36(1):01A104. https://doi.org/10.1116/1.5002667
22.
Aaltonen T, Ritala M, Sajavaara T, Keinonen J, Leskelä M. 2003. Atomic Layer Deposition of Platinum Thin Films. Chem. Mater.. 15(9):1924-1928. https://doi.org/10.1021/cm021333t
23.
Hagen DJ, Pemble ME, Karppinen M. 2019. Atomic layer deposition of metals: Precursors and film growth. 6(4): https://doi.org/10.1063/1.5087759
24.
Knoops HCM, Braeken EMJ, de Peuter K, Potts SE, Haukka S, Pore V, Kessels WMM. 2015. Atomic Layer Deposition of Silicon Nitride from Bis(tert-butylamino)silane and N2 Plasma. ACS Appl. Mater. Interfaces. 7(35):19857-19862. https://doi.org/10.1021/acsami.5b06833
25.
Gao Z, Banerjee P. 2019. Review Article: Atomic layer deposition of doped ZnO films. 37(5): https://doi.org/10.1116/1.5112777