assay
≥93% (complexometric)
form
powder (fine)
autoignition temp.
1400 °F
reaction suitability
reagent type: catalyst
core: aluminum
resistivity
2.6548 μΩ-cm
impurities
≤0.03% heavy metals (as Pb), ≤0.3% soluble in ether
bp
2460 °C (lit.)
mp
660.37 °C (lit.)
density
2.7 g/mL at 25 °C (lit.)
cation traces
Fe: ≤5000 mg/kg
SMILES string
[Al]
InChI
1S/Al
InChI key
XAGFODPZIPBFFR-UHFFFAOYSA-N
signalword
Danger
hcodes
存储类别
4.3 - Hazardous materials which set free flammable gases upon contact with water
wgk
nwg
flash_point_f
Not applicable
flash_point_c
Not applicable
Hazard Classifications
Flam. Sol. 1 - Water-react. 2
法规信息
新产品
此项目有
Structural features of oxide coatings on aluminum.
Keller F, et al.
Journal of the Electrochemical Society, 100(9), 411-419 (1953)
Electrochemistry of Cd (II) in the basic 1-ethyl-3-methylimidazolium chloride/tetrafluoroborate room temperature molten salt.
Chen P-Y and Sun I-W
Electrochimica Acta, 45(19), 3163-3170 (2000)
Aluminum ion diffusion in aluminum oxide.
Paladino AE and Kingery WD.
J. Chem. Phys. , 37(5), 957-962 (1962)
全球贸易项目编号
| 货号 | GTIN |
|---|---|
| 310069-25G | 04061826676592 |
| 700312-5ML | 04061832795485 |
| 747343-10ML | 04061837523274 |
| 747424-1ML | 04061837523366 |
| 725366-5ML | 04061832861494 |
| 725358-5ML | 04061832861487 |
| 51238-1ML | 04061837775208 |
| 518158-10G | 04061832542065 |
| 637106-250G | 04061832723600 |
| 790508-10ML | 04061837525148 |
| 310069-500G | 04061826676660 |
| 637106-25G | 04061832723679 |
| 637106-100G | 04061832723594 |
| 51238-5ML | 04061837775215 |
| 518158-50G | 04061832542072 |
| 747254-2ML | 04061837523113 |
| 747327-10ML | 04061837523212 |
| 747408-10ML | 04061832891699 |
| 747300-10ML | 04061837523137 |
| 747319-10ML | 04061837523175 |
| 700304-5ML | 04061832795454 |
| 700320-5ML | 04061832795492 |
| 725331-5ML | 04061832861470 |