grade
JIS special grade
assay
≥99.0%
form
solid
reaction suitability
reagent type: catalyst
core: iron
availability
available only in Japan
pH
1.5 (20 °C)
mp
47 °C (lit.)
SMILES string
O.O.O.O.O.O.O.O.O.[Fe+3].[O-][N+]([O-])=O.[O-][N+]([O-])=O.[O-][N+]([O-])=O
InChI
1S/Fe.3NO3.9H2O/c;3*2-1(3)4;;;;;;;;;/h;;;;9*1H2/q+3;3*-1;;;;;;;;;
InChI key
SZQUEWJRBJDHSM-UHFFFAOYSA-N
Still not finding the right product?
Explore all of our products under 硝酸铁(III) 九水合物
signalword
Danger
hcodes
Hazard Classifications
Eye Dam. 1 - Skin Corr. 1B
wgk
WGK 1
flash_point_f
Not applicable
flash_point_c
Not applicable
ppe
Eyeshields, Gloves, type P3 (EN 143) respirator cartridges
法规信息
新产品
此项目有
Runjuan Wang et al.
Bioresource technology, 120, 290-294 (2012-07-10)
The study investigated the effects of two-step pretreatment on fermentable sugar production from corn stalk silage. In the first step, the corn stalk silage was extracted by tepid water and then the solid was pretreated using Fe(NO(3))(3) as catalyst. The
Mara Ghiazza et al.
Chemical research in toxicology, 24(1), 99-110 (2010-12-22)
The mechanism of enhancement/inhibition of quartz toxicity induced by iron is still unclear. Here the amount of iron on a fibrogenic quartz (Qz) was increased by wet impregnation (Fe(NO(3))(3) 0.67 and 6.7 wt %). X-ray diffraction (XRD), XRF diffuse reflectance
Metal-mediated cross-linking in the generation of a marine-mussel adhesive.
Mary J Sever et al.
Angewandte Chemie (International ed. in English), 43(4), 448-450 (2004-01-22)